Vacuum bagging


Author
Message
SHaas
S
Supreme Being (533 reputation)Supreme Being (533 reputation)Supreme Being (533 reputation)Supreme Being (533 reputation)Supreme Being (533 reputation)Supreme Being (533 reputation)Supreme Being (533 reputation)Supreme Being (533 reputation)Supreme Being (533 reputation)
Group: Forum Members
Posts: 46, Visits: 384
Hi everybody,

I have all the time problems to get a perfect sealed vacuum bag. I think there was only one perfect bag in the last two months...

Now I am thinking about switching to an envelope bag in a pretty big size. I thought of backing the mould with breather to prevent little holes depending on the few sharp pieces on the backside. It also could be that the mould itself is not airtight because I had a crack to repair but I sprayed some layers of board sealer on the whole surface so it should be fine.

Anyone with experience on this or tips?
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search