Using epoxy + fibre glass to make mould for pre preg?


Author
Message
JamesC
JamesC
Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)
Group: Forum Members
Posts: 5, Visits: 138
Hi guys
Had a bit of a search + can't really find a yes or not
In light of unimould not being great for xpreg range my next mould I'll be making in epoxy to allow me to use the xpreg, building an oven at the moment which will have all the progressive temperature rise etc

My question is If I was to use epoxy with bidder bound Matt to make my mould, wet lay up then vac bagged to remove excess + oven cured, would they be suitable for xpreg or Not?
Purely to keep the mould costs down

Many thanks
James
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The most important thing to remember is use an epoxy gelcoat and resin that is suitable for the high temperature cures and also ensure you have done the full postcure cycle before using the moulds.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search