Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
I assume you mean 'powder' bound mat? If so, then yes, this combined with a high temperature epoxy laminating resin would be perfect. There's really no need to vacuum bag a mould though - you shouldn't be worried about the weight of the mould. Vacuum bagging moulds adds a whole new level of complications and really doesn't improve the final product at all, so just go with wet-lay for the moulds.
|