Newbie epoxy polishing problems
Newbie epoxy polishing problems
Post Reply
Like
2
Newbie epoxy polishing problems
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
myakpaul
m
myakpaul
posted 7 Years Ago
ANSWER
HOT
Topic Details
m
Group: Forum Members
Posts: 4,
Visits: 12
I have just finished my first epoxy coffee table and i sanded and polished it as per the video but it is coming up to a satin finish at best not a high gloss. what am i doing wrong?
Thanks in advance
Reply
Like
2
Reply
Bhamoggy
B
Bhamoggy
posted 7 Years Ago
ANSWER
Post Details
B
Group: Forum Members
Posts: 38,
Visits: 420
Hi
So table now done but struggling to get anywhere near the gloss finish that you see from the original pour before sanding. Have bought the NW1 to try but still a bit cloudy.
I applied the NW1 and used a polisher but on a slowish speed. Put the compound on and used polisher straight away. Have done this twice. Am I doing it wrong? Should I leave the NW1 on for a while before polishing? Not getting the expected results I’d hoped for as yet
match com delete account
Reply
Like
1
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Newbie epoxy polishing problems
myakpaul
-
7 Years Ago
Same here. Just completed first river table. Sanded down thru the grits to 2000. Using nanotech cut and polish 2 in 1 but can’t get a gloss finish. Still looks a Matt finish. ?Not sure what to do now
Bhamoggy
-
7 Years Ago
Glad its not just me! :) how big is your table?
myakpaul
-
7 Years Ago
First attempt so not gone too big. It’s 28” x 9 “ Not too happy with it at the moment. Think I expected a better finish than I’ve got so far. Here’s the top and reverse of the table. Trying to...
Bhamoggy
-
7 Years Ago
https://ibb.co/igKxwL https://ibb.co/cCqRqf
Bhamoggy
-
7 Years Ago
looks good. second photo has great depth of colour to it and nice grain to the wood. Thanks for sharing it
myakpaul
-
7 Years Ago
First attempt and not sure which side to have as top surface yet. Gonna use a clear gloss yacht varnish and see what it looks like after. Already preparing for second project. Gonna be a Brighton...
Bhamoggy
-
7 Years Ago
There is a bit of a technique to sanding, mostly cleanliness and ensuring you do not move up a grit until you are 100% sure you have removed the necessary scratches. Otherwise you will struggle to ge...
Warren (Staff)
-
7 Years Ago
Warren, Thanks for the info, just a couple of questions. What grit do i need to sand down too? Could you also explain what you mean by the polish breaking down? Do you mean that i need to polish for....
myakpaul
-
7 Years Ago
Minimum 1200 grit, ideally 1500 grit or better. You polish it for as long as it needs. Diminishing polishes you will feel it as they break down and move easier becoming finer. The shells look good,....
Warren (Staff)
-
7 Years Ago
Have done a 3mm pour having removed stones. Don’t want them coming straight thru the underside because of sanding. Will leave it 12hrs now then place the shells back as the resin should be tacky by.....
Bhamoggy
-
7 Years Ago
HiSo table now done but struggling to get anywhere near the gloss finish that you see from the original pour before sanding. Have bought the NW1 to try but still a bit cloudy. I applied the NW1 and.....
Bhamoggy
-
7 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search