Newbie epoxy polishing problems


Author
Message
myakpaul
m
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 4, Visits: 12
I have just finished my first epoxy coffee table and i sanded and polished it as per the video but it is coming up to a satin finish at best not a high gloss. what am i doing wrong?

Thanks in advance
Bhamoggy
B
Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)
Group: Forum Members
Posts: 38, Visits: 420
Same here.
Just completed first river table.
Sanded down thru the grits to 2000.
Using nanotech cut and polish 2 in 1 but can’t get a gloss finish. Still looks a Matt finish. ?
Not sure what to do now
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
There is a bit of a technique to sanding, mostly cleanliness and ensuring you do not move up a grit until you are 100% sure you have removed the necessary scratches.  Otherwise you will struggle to get a gloss finish at the end. Also bear in mind that many diminishing nano abrasives  (such as our NW1) will require a fair bit or working to break them down from the initially coarse compound into a finer polish.  If you polish it off too soon before the polish has broken down then the gloss will be poor.

Also be aware  to ensure you have left the resin long enough to cure in the first place.  We recommend a minimum of 48 hours at 20C before any sanding or shaping takes place - if your room cools over night, you might be trying to sand green resin which will always be difficult.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
myakpaul
m
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 4, Visits: 12
Warren (Staff) - 10/18/2018 8:16:59 AM
There is a bit of a technique to sanding, mostly cleanliness and ensuring you do not move up a grit until you are 100% sure you have removed the necessary scratches.  Otherwise you will struggle to get a gloss finish at the end. Also bear in mind that many diminishing nano abrasives  (such as our NW1) will require a fair bit or working to break them down from the initially coarse compound into a finer polish.  If you polish it off too soon before the polish has broken down then the gloss will be poor.

Also be aware  to ensure you have left the resin long enough to cure in the first place.  We recommend a minimum of 48 hours at 20C before any sanding or shaping takes place - if your room cools over night, you might be trying to sand green resin which will always be difficult.

Warren,
Thanks for the info, just a couple of questions. What grit do i need to sand down too? Could you also explain what you mean by the polish breaking down? Do you mean that i need to polish for longer with the polishing machine? if so how long do i need to polish for?

Thanks alot

Myak

myakpaul
m
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 4, Visits: 12
Bhamoggy - 10/17/2018 8:55:06 PM
Same here. Just completed first river table. Sanded down thru the grits to 2000. Using nanotech cut and polish 2 in 1 but can’t get a gloss finish. Still looks a Matt finish. ?Not sure what to do now

Glad its not just me! Smile
how big is your table?

Bhamoggy
B
Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)
Group: Forum Members
Posts: 38, Visits: 420
First attempt so not gone too big. It’s 28” x 9 “
Not too happy with it at the moment. Think I expected a better finish than I’ve got so far.
Here’s the top and reverse of the table.
Trying to upload pic but it won’t do it ???
Edited 7 Years Ago by Bhamoggy
Bhamoggy
B
Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)
Group: Forum Members
Posts: 38, Visits: 420
myakpaul
m
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 4, Visits: 12
Bhamoggy - 10/18/2018 7:28:39 PM

looks good. second photo has great depth of colour to it and nice grain to the wood. Thanks for sharing it

Bhamoggy
B
Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)
Group: Forum Members
Posts: 38, Visits: 420
First attempt and not sure which side to have as top surface yet. Gonna use a clear gloss yacht varnish and see what it looks like after.
Already preparing for second project.
Gonna be a Brighton beach table. Just laid out in preparation. Will do 3mm first pour hopefully tomorrow.
What do you think of this?




Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Minimum 1200 grit, ideally 1500 grit or better.  You polish it for as long as it needs. Diminishing polishes you will feel it as they break down and move easier becoming finer.

The shells look good, but you may need to secure it all down with a thin layer of resin to avoid things floating away. 


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search