Newbie epoxy polishing problems


Author
Message
myakpaul
m
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 4, Visits: 12
I have just finished my first epoxy coffee table and i sanded and polished it as per the video but it is coming up to a satin finish at best not a high gloss. what am i doing wrong?

Thanks in advance
Replies
myakpaul
m
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 4, Visits: 12
Bhamoggy - 10/17/2018 8:55:06 PM
Same here. Just completed first river table. Sanded down thru the grits to 2000. Using nanotech cut and polish 2 in 1 but can’t get a gloss finish. Still looks a Matt finish. ?Not sure what to do now

Glad its not just me! Smile
how big is your table?

Bhamoggy
B
Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)
Group: Forum Members
Posts: 38, Visits: 420
First attempt so not gone too big. It’s 28” x 9 “
Not too happy with it at the moment. Think I expected a better finish than I’ve got so far.
Here’s the top and reverse of the table.
Trying to upload pic but it won’t do it ???
Edited 7 Years Ago by Bhamoggy
Bhamoggy
B
Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)
Group: Forum Members
Posts: 38, Visits: 420
myakpaul
m
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 4, Visits: 12
Bhamoggy - 10/18/2018 7:28:39 PM

looks good. second photo has great depth of colour to it and nice grain to the wood. Thanks for sharing it

Bhamoggy
B
Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)Supreme Being (288 reputation)
Group: Forum Members
Posts: 38, Visits: 420
First attempt and not sure which side to have as top surface yet. Gonna use a clear gloss yacht varnish and see what it looks like after.
Already preparing for second project.
Gonna be a Brighton beach table. Just laid out in preparation. Will do 3mm first pour hopefully tomorrow.
What do you think of this?




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
myakpaul - 7 Years Ago
Bhamoggy - 7 Years Ago
myakpaul - 7 Years Ago
Bhamoggy - 7 Years Ago
                     https://ibb.co/igKxwL https://ibb.co/cCqRqf
Bhamoggy - 7 Years Ago
myakpaul - 7 Years Ago
Bhamoggy - 7 Years Ago
Warren (Staff) - 7 Years Ago
myakpaul - 7 Years Ago
Warren (Staff) - 7 Years Ago
Bhamoggy - 7 Years Ago
Bhamoggy - 7 Years Ago