Same here.
Just completed first river table.
Sanded down thru the grits to 2000.
Using nanotech cut and polish 2 in 1 but can’t get a gloss finish. Still looks a Matt finish. ?
Not sure what to do now
myakpaul
m
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 4, Visits: 12
I have just finished my first epoxy coffee table and i sanded and polished it as per the video but it is coming up to a satin finish at best not a high gloss. what am i doing wrong?

Thanks in advance
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search