Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Projects
»
Motorsport, Vehicle Design and Modification
»
New Project : TM 250 2T > Plastic kit to Carbon
New Project : TM 250 2T > Plastic kit to Carbon
Post Reply
Like
8
New Project : TM 250 2T > Plastic kit to Carbon
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Thanasis
Thanasis
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 36,
Visits: 234
This time I didn't want to turn the bike black (original colour was white). So for first layer i use 200gr Alufibre (Silver Glass) and the rest 200 gr CF.
The 200 gr Alufibre turned to be very difficult to work with since it is very delicate and it is to destroy the weave. It is easy to have cosmetic issues in your final product. Possible the 290 gr version could be easier to work with and give better visual appearance but wouldn't help keeping the weight low.
Project is currently near completion.
Side panel and rear fender:
Front number plate and fender:
More photos to come with more details on the project.
Edited
8 Years Ago by
Thanasis
Reply
Like
8
Replies
Melvin Meppelink
Melvin Meppelink
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 23
what kind of tooling gelcoat do you use?
Reply
Like
8
Thanasis
Thanasis
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 36,
Visits: 234
+
x
Melvin Meppelink - 11/4/2018 12:45:54 PM
what kind of tooling gelcoat do you use?
I use Vinylester Gelcoat from Polyprocess (a French company that has a distributor here in Athens) and then Vinylester Distitron from same company for the layers of CSM. All applied with brush.
For in mould gelcoat I spray uncoloured Vinylester gelcoat compatible with epoxy.
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
New Project : TM 250 2T > Plastic kit to Carbon
Izo78
-
8 Years Ago
From yesterday, ready to demould the radiator cover, Looking good The most messy part of carbon making is following next, cutting the part in shape and paying attention not to over do it and ruin...
Izo78
-
8 Years Ago
good work, i always like seeing the tool as well as the parts!
scottracing
-
8 Years Ago
Looks very good man, nice to see that there are also other motocross enthusiasts (i ride a yz450f 18). keep up the good work
MM-Composites
-
8 Years Ago
Thanks! I ride both the TM and the MXV! Different worlds though : )
Izo78
-
8 Years Ago
what kind of tooling gelcoat do you use?
MM-Composites
-
8 Years Ago
I use Vinylester Gelcoat from Polyprocess (a French company that has a distributor here in Athens) and then Vinylester Distitron from same company for the layers of CSM. All applied with brush. For i...
Izo78
-
8 Years Ago
Radiator covers finished and installed on the bike : Close up look of the weave :
Izo78
-
8 Years Ago
Project is finished long time ago, finally I was able to upload some more photos. Clear background stickers were designed for this project in order to have a better visual appearance. The only.....
Izo78
-
7 Years Ago
Back to black! A new kit for TM 2t 250-300 MY'15-19 completed. Resin infused with epoxy fatigue and inmould gelcoated with clear EPX Iso Npg. Weight reduction -605 gr from original plastic kit....
Izo78
-
7 Years Ago
A small walk around clip of the carbon parts installed in the bike.
Izo78
-
7 Years Ago
Looking really good! You can see a lot of effort has gone into the parts!
Warren (Staff)
-
7 Years Ago
Thank you Warren for your kind remarks!
Izo78
-
7 Years Ago
dude epic!!! where is the mxv :(
Thomb
-
7 Years Ago
Still got it, don't worry ; )
Izo78
-
7 Years Ago
Man this is crazy! Wonderful job! I am on your way, the only difference is that I have a gixer 600 K5... :laugh:
Legoman
-
7 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search