Hi 

 Has anyone had any problems with pigments in PU resin loosing colour and becoming patchy over time? I am using Xencast toughened P6 with EC pigments, no fillers, mech mixed, de-gassed the parts are nice colourful and shiny when they come out the mould, after a few days the colour is dying back but the parts are still nice and glossy.

 Any help would be appreciated.

Thanks
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Have you tried a small experiment in warmer curing conditions to see if it still happens? 


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Sparky2305 - 7 Years Ago
Hanaldo - 7 Years Ago
Warren (Staff) - 7 Years Ago
Sparky2305 - 7 Years Ago
Sparky2305 - 7 Years Ago
Warren (Staff) - 7 Years Ago
Sparky2305 - 7 Years Ago
Warren (Staff) - 7 Years Ago
Sparky2305 - 7 Years Ago
Warren (Staff) - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search