Hi
Has anyone had any problems with pigments in PU resin loosing colour and becoming patchy over time? I am using Xencast toughened P6 with EC pigments, no fillers, mech mixed, de-gassed the parts are nice colourful and shiny when they come out the mould, after a few days the colour is dying back but the parts are still nice and glossy.
Any help would be appreciated.
Thanks
|