Hi 

 Has anyone had any problems with pigments in PU resin loosing colour and becoming patchy over time? I am using Xencast toughened P6 with EC pigments, no fillers, mech mixed, de-gassed the parts are nice colourful and shiny when they come out the mould, after a few days the colour is dying back but the parts are still nice and glossy.

 Any help would be appreciated.

Thanks
Reply
Sparky2305
Sparky2305
Supreme Being (91 reputation)Supreme Being (91 reputation)Supreme Being (91 reputation)Supreme Being (91 reputation)Supreme Being (91 reputation)Supreme Being (91 reputation)Supreme Being (91 reputation)Supreme Being (91 reputation)Supreme Being (91 reputation)
Group: Forum Members
Posts: 10, Visits: 69
Sorry for the delay Warren this is how it tends to go, It's not as prominent in the pic but it can be seen, as I say they start off all jet black, 8% is the ratio I am using.

Cheers



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Sparky2305 - 7 Years Ago
Hanaldo - 7 Years Ago
Warren (Staff) - 7 Years Ago
Sparky2305 - 7 Years Ago
Sparky2305 - 7 Years Ago
Warren (Staff) - 7 Years Ago
Sparky2305 - 7 Years Ago
Warren (Staff) - 7 Years Ago
Sparky2305 - 7 Years Ago
Warren (Staff) - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search