Hi,

We offer a very similar high quality PU Fast Cast which is especially good for fine detail reproduction and fast  curing.  Pot life is typically 2.5-3 mins.  You can fine our P2 Fast Cast here: Xencast P2 Fast Cast Polyurethane Casting Resin


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Dessert Mix
Dessert Mix
Supreme Being (294 reputation)Supreme Being (294 reputation)Supreme Being (294 reputation)Supreme Being (294 reputation)Supreme Being (294 reputation)Supreme Being (294 reputation)Supreme Being (294 reputation)Supreme Being (294 reputation)Supreme Being (294 reputation)
Group: Forum Members
Posts: 24, Visits: 69
The G26 of SIKA is a fast cast polyurethane resin, it sets very fast, maybe three minutes and its is very liquid. But I am looking for an option.
Any clue is welcome!!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search