Dessert Mix
Dessert Mix
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 24,
Visits: 69
The G26 of SIKA is a fast cast polyurethane resin, it sets very fast, maybe three minutes and its is very liquid. But I am looking for an option.
Any clue is welcome!!
Reply
Like
5
Warren (Staff)
Warren (Staff)
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Hi,
We offer a very similar high quality PU Fast Cast which is especially good for fine detail reproduction and fast curing. Pot life is typically 2.5-3 mins. You can fine our P2 Fast Cast here:
Xencast P2 Fast Cast Polyurethane Casting Resin
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search