By Dessert Mix - 11/2/2018 12:21:12 PM
The G26 of SIKA is a fast cast polyurethane resin, it sets very fast, maybe three minutes and its is very liquid. But I am looking for an option. Any clue is welcome!!
|
By Warren (Staff) - 11/2/2018 5:05:09 PM
Hi,
We offer a very similar high quality PU Fast Cast which is especially good for fine detail reproduction and fast curing. Pot life is typically 2.5-3 mins. You can fine our P2 Fast Cast here: Xencast P2 Fast Cast Polyurethane Casting Resin
|
|