I've got a kg of EL80 and I've been having a little play with some offcuts of cloth to see how it cures.  One thing I did notice is that its fairly viscous.  Is it OK to warm it a touch to thin it down a bit?

Would a review of my test pieces be of use?  If so I'd appreciate a few pointers of what people woould like to see.
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
thanks for that information! could you add some pictures to show how it bends and how it looks? Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
FLD - 14 Years Ago
FLD - 14 Years Ago
Matt (Staff) - 14 Years Ago
FLD - 14 Years Ago
FLD - 14 Years Ago
matthieutje65 - 14 Years Ago
FLD - 14 Years Ago
FLD - 14 Years Ago
Matt (Staff) - 14 Years Ago
FLD - 14 Years Ago
FLD - 14 Years Ago
Matt (Staff) - 14 Years Ago
FLD - 12 Years Ago
Warren (Staff) - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search