I've got a kg of EL80 and I've been having a little play with some offcuts of cloth to see how it cures.  One thing I did notice is that its fairly viscous.  Is it OK to warm it a touch to thin it down a bit?

Would a review of my test pieces be of use?  If so I'd appreciate a few pointers of what people woould like to see.
Reply
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Matt (Staff) (17/12/2012)
Hi FLD,

Thanks for the picture; it sound look like the 'bulging tow' has been caused by being flexed when not fully cured. It appears that some of the carbon tows have been able to break free of the matrix and then not bedded back down afterwards (which is not a huge surprise if the resin was mostly cured by then). Once it's properly cured you should not be able to do anything like this - we have samples that get mauled quite a bit as demonstration pieces and they hold up well. Thank you for the post and I look forward to hearing how the part performs in use.

All the best, Matt


I completely agree.  Operator error!  I was too keen to see how flexible it was.  My splitter has come out just fine.  I'll post up some pics of the final piece later. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
FLD - 13 Years Ago
FLD - 13 Years Ago
Matt (Staff) - 13 Years Ago
FLD - 13 Years Ago
FLD - 13 Years Ago
matthieutje65 - 13 Years Ago
FLD - 13 Years Ago
FLD - 13 Years Ago
Matt (Staff) - 13 Years Ago
FLD - 13 Years Ago
FLD - 13 Years Ago
Matt (Staff) - 13 Years Ago
FLD - 11 Years Ago
Warren (Staff) - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search