I've got a kg of EL80 and I've been having a little play with some offcuts of cloth to see how it cures.  One thing I did notice is that its fairly viscous.  Is it OK to warm it a touch to thin it down a bit?

Would a review of my test pieces be of use?  If so I'd appreciate a few pointers of what people woould like to see.
Replies
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Dont worry, I've had a play and answered my own question.  Yes you can stand the mixing cup in warm water to thin it a touch.  It does go incredibly thick as the temp drops!
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi, yes, you're dead-right. The EF80 does start off life pretty thick but this viscosity (as with all epoxies) can be lowered by warming it, if necessary.

Let us know how you get on with it!

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
FLD - 13 Years Ago
FLD - 13 Years Ago
Matt (Staff) - 13 Years Ago
FLD - 13 Years Ago
FLD - 13 Years Ago
matthieutje65 - 13 Years Ago
FLD - 13 Years Ago
FLD - 13 Years Ago
Matt (Staff) - 13 Years Ago
FLD - 13 Years Ago
FLD - 13 Years Ago
Matt (Staff) - 13 Years Ago
FLD - 11 Years Ago
Warren (Staff) - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search