		| By FLD - 10/8/2012 7:05:25 PM 
 I've got a kg of EL80 and I've been having a little play with some offcuts of cloth to see how it cures.  One thing I did notice is that its fairly viscous.  Is it OK to warm it a touch to thin it down a bit?
 
 Would a review of my test pieces be of use?  If so I'd appreciate a few pointers of what people woould like to see.
 |  
		| By Warren (Staff) - 11/4/2014 11:13:29 AM 
 Good to see it holds up quite well.
 |  |