Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Well realistically its only a surface coat, it's not doing anything for the structural integrity of the part. But it can also affect the surface finish, which is why I dont do it. But the idea is that you only apply a very fine mist, just to break the surface tension that is holding the bubbles. If you apply too much, then it can cause issues. But it's the same if you're using a heat gun, you can burn the surface if you're not careful, so theres risks with everything - just takes practice to get good at whatever method youre using.
|