By Furrari - 9/26/2018 12:15:39 PM

I have just watched a vid on YouTube where a man was doing a wet layup. He did the first couple of coats of resin in the usual way but on the last two coats he sprayed them with a light coat of acetone. He said it gave a better final finish. Anybody know anything about this?

Mick
By Warren (Staff) - 9/27/2018 9:26:24 AM

In theory the thin mist will have long evaporated off the surface of the resin before it can cause any damage.