Hi every one.

Can I skin plastic part with prepreg CF(X C 1 10) instead of wet layup? ,I intend to do skinning for plastic parts at low temp cure 85c degree ,because I need to keep the weave in line..
Thanks


Reply
dinh gia truyen
dinh gia truyen
Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)
Group: Forum Members
Posts: 6, Visits: 34
Warren (Staff) - 9/18/2018 10:06:03 AM
You would get a very poor cosmetic finish that is assuming the plastic can take the heat. 85C is a low temperature cure.  If you have to add multiple layers of resin anyway then don't waste the expense of the Pre-preg when a stabilised fabric will do fine at holding the weave alignment.  YOu can find our ProFinish fabric here: ProFinish Carbon Fibre 2/2 Twill 3k 210g

Dear Warren,

Many thank you for your advice,
I have ProFinish Carbon Fiber Cloth 2/2 Twill, which was from Easycomposite and i intend to use for these parts also,
But my parts have no smooth surface ( 2 mouting points),,and i think it will effect to the weave appearance at these areas,so i plan to use the XC110,.
and i will do the same process for prepreg ,i will devide and cut the prepreg according to the actual mouting points shape ,then use vacumm bag with oven,.for the finish i will aplly multiple  wet epoxy to get the finish ,

Please help comment on my above plan if available.
Thank you
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search