dinh gia truyen
dinh gia truyen
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 6,
Visits: 34
Hi every one.
Can I skin plastic part with prepreg CF(X C 1 10) instead of wet layup? ,I intend to do skinning for plastic parts at low temp cure 85c degree ,because I need to keep the weave in line..
Thanks
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Skinning plastic with prepreg CF
dinh gia truyen
-
8 Years Ago
You would get a very poor cosmetic finish that is assuming the plastic can take the heat. 85C is a low temperature cure. If you have to add multiple layers of resin anyway then don't waste the expens...
Warren (Staff)
-
8 Years Ago
Dear Warren, Many thank you for your advice, I have ProFinish Carbon Fiber Cloth 2/2 Twill, which was from Easycomposite and i intend to use for these parts also, But my parts have no smooth surface...
dinh gia truyen
-
8 Years Ago
Plastic parts are going to soften and deform a lot with the heat and vacuum, you will end up with them being totally the wrong shape. I would rethink your approach - pre-preg isn't the material for....
Hanaldo
-
8 Years Ago
Hi,Hanaldo, Thank you so much for your advise, I 'm still thinking Thank you
dinh gia truyen
-
8 Years Ago
You can use a spray adhesive such as 3M Super 77 to keep the dry fabric in place on the part and apply resin over. Another method is to apply the resin over the fabric on a flat surface and leave it....
ISCmech-composite
-
8 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search