Kayak polo paddle repair


Author
Message
javier
javier
Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)
Group: Forum Members
Posts: 7, Visits: 36
HÍ'm writing from Spain.

I need some help to fix up a Kayak Polp paddel. Ih has a yellow band surrounding it all that it's suposed to be a Kevlar textil band fixed with epoxi.

I've found the Video "How to Repair a Damaged Composite Canoe or Kayak" and I thought I may find help here Wink

Could you please help me with the right choice of the materiarls I may need?

 

Thank you very much.

 

Javier
Replies
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Quantity is the length in metres that you want. I would think either 1m or 2m would be fine. Just measure the circumference of the blade edge and multiply it by 2 (for both blades).

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
javier
javier
Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)
Group: Forum Members
Posts: 7, Visits: 36
Let's go!!

Thank you.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
javier - 14 Years Ago
Matt (Staff) - 14 Years Ago
Matt (Staff) - 14 Years Ago
javier - 14 Years Ago
Matt (Staff) - 14 Years Ago
javier - 14 Years Ago
javier - 14 Years Ago
Matt (Staff) - 14 Years Ago
                 Let's go!! Thank you.
javier - 14 Years Ago
javier - 14 Years Ago
Matt (Staff) - 14 Years Ago
javier - 14 Years Ago

Similar Topics