By javier - 10/1/2012 10:19:45 AM				
            
                      
            HÍ'm writing from Spain.
  I need some help to fix up a Kayak Polp paddel. Ih has a yellow band surrounding it all that it's suposed to be a Kevlar textil band fixed with epoxi.
  I've found the Video "How to Repair a Damaged Composite Canoe or Kayak" and I thought I may find help here  
  Could you please help me with the right choice of the materiarls I may need?
   
  Thank you very much.
   
  Javier
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By javier - 10/31/2012 7:41:55 AM				
            
                      
            Hi,
  Definitely the workshop temperature was the problem. I placed the paddle in a smaller room with a little electric heater and it worked perfectly.
  Thank you again for your help.
  Javier.
           
		 | 			
		 
	
	
						
		 	
		
	 |