Looks like it could be a nightmare!
If you can CNC a core , then you can use that to make a mould and then work from there.
Making the wooden core would be a case of using thin strips of wood bonded together - using the mould as a template. The strips would need to be thin enough to easily curve around. You would clamp it top and bottom and in various places then build up the strips of wood to get the shaped core in wood.
Once youve done that, the infusion would be simple by comparison!
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|