Dear easycomposites,

I intend to do this Project, i was planning to do it withlike the skateboard tutorial you have on YouTube… just with thinner wood.

Do you have any ideas on how much layers i would probably Need?I was wondering also how the Wood could bend in future?? It should stay in hisshape.

The Rhino object would be my mould. Thickness, i dont know, probably 5-7mm?
Thanks alot! Franzis

  

By Franz Mussner - 11/7/2018 1:37:58 PM


hope to explain it with the image better