I am researching the most economical way for us to source carbon fiber pre-preg for our prototyping shop. I was wondering if there are any cross-compatibility issues I need to be aware of when it comes to laminating prepregs from multiple suppliers. Specifically, I want to cure UF3325 TCR™ RESIN from Composite Envisions with Easy Composites' XPreg XC110 Resin. Is there an easy way to tell if these epoxies are compatible?

Thanks,

Nathan
Replies
scottracing
scottracing
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
f1rob - 9/6/2018 12:00:27 PM
Steve Broad - 9/6/2018 10:49:44 AM
f1rob - 9/6/2018 9:21:42 AM
As others have said sucking and see
Most will work together no problem
At the moment am doing some f1 pod fronts
6 different materials (1 glass 5 carbon)
Woven an ud 
4 different weaves
3 different resin systems
Works fine

Very interesting. Why are you having to use different resin systems (apart from because of glass and carbon)?

Most teams can't get all their materials from one supplier

That an young composite designers like to appear really clever an inventive an make it as complicated as possible
Lot to be said for KISS
but no we have a part with flat tow,u/d,glass,satin weave an 2x2 twill all for a bit of bodywork !

Its all about making it as complicated and expensive in f1 lol.


f1rob
f1rob
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
You know it mate 😊
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
nreindel - 6 Years Ago
Steve Broad - 6 Years Ago
Hanaldo - 6 Years Ago
SleepingAwake - 6 Years Ago
Steve Broad - 6 Years Ago
nreindel - 6 Years Ago
Warren (Staff) - 6 Years Ago
Fasta - 6 Years Ago
f1rob - 6 Years Ago
Steve Broad - 6 Years Ago
f1rob - 6 Years Ago
Steve Broad - 6 Years Ago
f1rob - 6 Years Ago
                             Glass as in glass or, as I thought, fibreglass?
Steve Broad - 6 Years Ago
                                 Pre preg glassYou haven't seen grp in f1 for about 30 yrs
f1rob - 6 Years Ago
                                     So what is it actually made from?
Steve Broad - 6 Years Ago
f1rob - 6 Years Ago
                     Its all about making it as complicated and expensive in f1 lol.
scottracing - 6 Years Ago
                         You know it mate 😊
f1rob - 6 Years Ago
nreindel - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search