Group: Forum Members
Posts: 8,
Visits: 145
|
Thanks for the replies, folks! It looks like the best course of action is to first make sure the cure profiles for the prepregs are as similar as possible. If they are, I'll give them a test and see how they work together. If they delaminate, the epoxies are clearly not compatible, but are there any other less obvious compatibility issues I need to be looking for?
|