Group: Forum Members
Posts: 550,
Visits: 27K
|
Sorry, it should be an oil bathed Rotary vane. The bigger one is oil free. Which means that the vacuum level is not good enough for resin infusion. For vacuum compression it should be ok, though. so overkill, no, not by any means except maybe volume flow. But for 500$ you can allmost get an dvp ec 20, wich would be overkill, and which got even better volume flow. Or almost 5 cheap oil bathed vacuum pumps, wich will each suit your needs.
|