By Otolithco - 6/28/2018 6:08:51 PM
Gast DOA-P707-FB listed at $200 obo
 Gast 2067-v108 listed at $500 obo
 These pumps are available locally and are new.
Anyone have experience with these pumps? Would they be suitable for composites? My parts are going to be in bag rather than a mold. Parts are roughly 5' long by 6" wide.
Any help would be appreciated.
Thanks
|
By Steve Broad - 7/31/2018 10:04:14 PM
I use EC's pump and it works fine. Pulled a good vacuum on my car's front clip (around 1.6m x 1.6m x 0.6m) so will cope with most things.
|
|