Stickers between layers


Author
Message
Furrari
F
Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)
Group: Awaiting Activation
Posts: 63, Visits: 99
Hanaldo.
Hi. Yes that be an idea but the carbon/twaron is already on order. I’ve also seen some carbon finish stitched together to form a V. Anyway as I say, I’m a total novice on this subject and I think I’ve thrown myself in at the deep end, You soon learn with this method. I’ve also found a couple of small jobs as practice.
New materials and working methods are fun aren’t they.

Mick
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh don't get me wrong, I wasnt necessarily recommending the ProFinish! I was just pointing out it was more likely that Jas meant that than pre-preg.

Personally, I don't actually like set-weave carbon. You can achieve virtually the exact same thing by misting a coat of spray adhesive over the back of regular carbon and letting it dry before using it. Or if you want a really stable material, use spray adhesive to stick two layers of regular material together. 
Furrari
F
Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)
Group: Awaiting Activation
Posts: 63, Visits: 99
Hanaldo - 6/21/2018 2:00:12 AM
Yeh don't get me wrong, I wasnt necessarily recommending the ProFinish! I was just pointing out it was more likely that Jas meant that than pre-preg.

Personally, I don't actually like set-weave carbon. You can achieve virtually the exact same thing by misting a coat of spray adhesive over the back of regular carbon and letting it dry before using it. Or if you want a really stable material, use spray adhesive to stick two layers of regular material together. 



Furrari
F
Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)
Group: Awaiting Activation
Posts: 63, Visits: 99
Hanaldo.
No problems. Thanks for the info, I welcome any input. I hadn’t realised that the pro-finish had the antifray finish. As I write the printer is making some brackets for storing roles of fabrics off the floor.

The excitement of starting lay ups is rising.

Mick
Furrari
F
Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)
Group: Awaiting Activation
Posts: 63, Visits: 99
I bought a set of sample weaves (7 of them) of CF. I used fusion fix to stick them to a piece of ABS andlayered them up with XCR resin mixed 3:1 by weight. Over this I layed peel ply ( white with the black lines) a layer of breather cloth ( white fluffy stuff) and a layer of vacuum ply ( the pink stuff). Vacuumed it at 80% vacuum for about 2hours and then let it set overnight.

Tried to remove all the bagging material this morning and all the samples came off with the peel ply. It’s come off giving a very smooth finish to the CF which I’m going to put more resin on to see the finish.

Anybody know why.? Had I sanded the ABS too well (600 grit),? Does the resin not stick well to ABS ? Were the gods of composites against me. Please help.
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Were you trying to bond them to the ABS? ABS isn't an easy plastic to bond to, you would need to aggressively stand it with 60 or 80 grit to get any sort of bond. Even then, you would likely find you could pry them off quite easily if you tried.

Just a side note; 80% vacuum with no perforated release film is quite high, you will likely leave your laminate quite dry. You should add a layer of perforated release film after the peel ply, and consider dropping your vacuum level a bit if cosmetics are more critical than weight.
Furrari
F
Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)
Group: Awaiting Activation
Posts: 63, Visits: 99
Hanaldo - 6/24/2018 10:59:27 PM
Were you trying to bond them to the ABS? ABS isn't an easy plastic to bond to, you would need to aggressively stand it with 60 or 80 grit to get any sort of bond. Even then, you would likely find you could pry them off quite easily if you tried.

Just a side note; 80% vacuum with no perforated release film is quite high, you will likely leave your laminate quite dry. You should add a layer of perforated release film after the peel ply, and consider dropping your vacuum level a bit if cosmetics are more critical than weight.



Furrari
F
Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)
Group: Awaiting Activation
Posts: 63, Visits: 99
Hanaldo. Thanks for that info. I was coming to these conclusions myself but it’s good to have some input from those more experienced than me (and that’s just about everybody).

Mick
Jas1712
J
Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)
Group: Forum Members
Posts: 6, Visits: 69
Hanaldo - 6/19/2018 2:42:33 PM
I think Jas may have actually meant the ProFinish carbon rather than pre-preg as he mentions using spray adhesive with it which would be totally unnecessary and even detrimental with pre-preg.

The ProFinish is a set weave carbon, which is a type of dry carbon fabric that has a binder in it to prevent the fibres from fraying as much and keeping the weave neat. It can be more accurately than regular dry carbon, so can be great for doing v-weaves in an infusion or wet lay setup.

Yes you're right I meant the pro finish oneI will get it the next week, thanks for get it clear.
Cheers and good luck with your project.

Jas1712
J
Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)
Group: Forum Members
Posts: 6, Visits: 69
Jas1712 - 6/25/2018 4:35:01 PM
Hanaldo - 6/19/2018 2:42:33 PM
I think Jas may have actually meant the ProFinish carbon rather than pre-preg as he mentions using spray adhesive with it which would be totally unnecessary and even detrimental with pre-preg.

The ProFinish is a set weave carbon, which is a type of dry carbon fabric that has a binder in it to prevent the fibres from fraying as much and keeping the weave neat. It can be more accurately than regular dry carbon, so can be great for doing v-weaves in an infusion or wet lay setup.

Yes you're right I meant the pro finish oneI will get it the next week, thanks for get it clear.
Cheers and good luck with your project.

I knew aboya the profinish one when it was to late, i ordered the started kit and the tank required the pro finish one afortunately could save my project  but definitely I will try it in my next project 