Hi,
Im jut about to skinning some part from my motorcycle, my cuestion is that I can apply some stickers before the final coat, like the Ducati and some lines.
This is a great place, congrats for the great job that you're doing.
Furrari
F
Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)Supreme Being (782 reputation)
Group: Awaiting Activation
Posts: 63, Visits: 99
Executive decision taken. One of the badges is going but I hope to recycle the other. Going for the hole with backing method. All the stuff for vacuum bagging ordered apart from the CF and the pump. ( just waiting to establish the threads on the pump). I have ordered 8 different samples of CF to see what I like. Also got to order the Ferrari stickers ( big yellow ones to match the car). I’ll post pictures before I start work.

M
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I think Jas may have actually meant the ProFinish carbon rather than pre-preg as he mentions using spray adhesive with it which would be totally unnecessary and even detrimental with pre-preg.

The ProFinish is a set weave carbon, which is a type of dry carbon fabric that has a binder in it to prevent the fibres from fraying as much and keeping the weave neat. It can be more accurately than regular dry carbon, so can be great for doing v-weaves in an infusion or wet lay setup.