Two part bonding expoxy


Author
Message
mwr2452
mwr2452
Supreme Being (113 reputation)Supreme Being (113 reputation)Supreme Being (113 reputation)Supreme Being (113 reputation)Supreme Being (113 reputation)Supreme Being (113 reputation)Supreme Being (113 reputation)Supreme Being (113 reputation)Supreme Being (113 reputation)
Group: Forum Members
Posts: 15, Visits: 28
Is the Permabond 2 part 515 usable for parts made out of vinyl esters resin as well? Or only epoxy resin compatible?
Replies
Paul (Staff)
Paul (Staff)
Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)
Group: Administrators
Posts: 134, Visits: 614
Hi,

The Permabond 515 will bond vinylester parts very well, obviously you would need to prepare the area like any other (sand and degrease)

As a rule of thumb these guidlines can be followed for resin bonding;

Epoxy will bond well to cured polyester/vinylester
Vinylester/polyester will bond reasonably well to itself
Vinylester/polyester will not bond well to cured epoxy
Epoxy will bond well to itself

The ET515 is an epoxy based adhesive so it should adhere well to any resin system.

Paul Statham
Easy Composites / Carbon Mods - Technical
mwr2452
mwr2452
Supreme Being (113 reputation)Supreme Being (113 reputation)Supreme Being (113 reputation)Supreme Being (113 reputation)Supreme Being (113 reputation)Supreme Being (113 reputation)Supreme Being (113 reputation)Supreme Being (113 reputation)Supreme Being (113 reputation)
Group: Forum Members
Posts: 15, Visits: 28
Thank you Paul!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search