Dyneema


Author
Message
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
Any one using a dyneema pre preg ?
What's your max cure temp before you affect the performance of the cloth ???
Cheers
Reply
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
oekmont - 4/26/2018 11:20:39 AM
Dyneema indeed got a very low temperature resistance. But this seems more of a question for the manufacturer of the prepreg.

So you go by what the manufacturer recommends :-)

Edited 7 Years Ago by Steve Broad