Any one using a dyneema pre preg ?
What's your max cure temp before you affect the performance of the cloth ???
Cheers
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Dyneema
f1rob
-
8 Years Ago
I would have thought that your temp is governed by the resin rather than the cloth?
Steve Broad
-
8 Years Ago
Dyneema indeed got a very low temperature resistance. But this seems more of a question for the manufacturer of the prepreg.
oekmont
-
8 Years Ago
So you go by what the manufacturer recommends :-)
Steve Broad
-
8 Years Ago
Only used it a few times over the years Was always told that as it's a Palomar construction that 80 was the max cure temp above 85 it starts to loose it's ballistic characteristics ? Doing samples...
f1rob
-
8 Years Ago
rob i will have a chat with the materials team here at work and see if they know anything.
scottracing
-
8 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search