Epoxy Glass Finish and then Varnish


Author
Message
Rek
R
Rek
posted 7 Years Ago HOT
Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)
Group: Forum Members
Posts: 3, Visits: 3
Hi

I used your Glass Coat Epoxy two part for the restoration of my classic car dashboard.

It worked well.

First coating - bought up some fibres from the new veneer. Sand and second coat - perfect, until someone (probably me) opened a door and dust settled on the second coat creating small dimples.

Can I sand this and finish with a varnish - something like a yacht varnish? I don't want to add a further coat or the finish will make the coating look too deep.

Guy
 



Reply
Rek
R
Rek
posted 7 Years Ago HOT
Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)
Group: Forum Members
Posts: 3, Visits: 3
Hanaldo - 4/20/2018 2:29:07 PM
EC's NW1 cutting compound is far and above the best product I've ever used.

OK -I will take a look 

Thanks