By Rek - 4/19/2018 4:24:26 PM
Hi
I used your Glass Coat Epoxy two part for the restoration of my classic car dashboard.
It worked well.
First coating - bought up some fibres from the new veneer. Sand and second coat - perfect, until someone (probably me) opened a door and dust settled on the second coat creating small dimples.
Can I sand this and finish with a varnish - something like a yacht varnish? I don't want to add a further coat or the finish will make the coating look too deep.
Guy
|
By Warren (Staff) - 4/20/2018 4:33:15 PM
As Hanaldo states, NW1 White Super Cutting Compoundis the one we recommends as it works very well
|
|