Hi
I used your Glass Coat Epoxy two part for the restoration of my classic car dashboard.
It worked well.
First coating - bought up some fibres from the new veneer. Sand and second coat - perfect, until someone (probably me) opened a door and dust settled on the second coat creating small dimples.
Can I sand this and finish with a varnish - something like a yacht varnish? I don't want to add a further coat or the finish will make the coating look too deep.
Guy
|