Epoxy Glass Finish and then Varnish
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Rek
R
Rek
posted 7 Years Ago
ANSWER
HOT
Topic Details
R
Group: Forum Members
Posts: 3,
Visits: 3
Hi
I used your Glass Coat Epoxy two part for the restoration of my classic car dashboard.
It worked well.
First coating - bought up some fibres from the new veneer. Sand and second coat - perfect, until someone (probably me) opened a door and dust settled on the second coat creating small dimples.
Can I sand this and finish with a varnish - something like a yacht varnish? I don't want to add a further coat or the finish will make the coating look too deep.
Guy
Reply
Like
3
Reply
Warren (Staff)
Warren (Staff)
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
As Hanaldo states,
NW1 White Super Cutting Compoundis the one we recommends as it works very well
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Epoxy Glass Finish and then Varnish
Rek
-
7 Years Ago
Yes you can do that. Alternatively sand off the dust dimples then work back up the grits to 1500 again and polish it back to a high gloss.
Warren (Staff)
-
7 Years Ago
Thanks Warren - that might be easier. What polishing compound would you recommend? Its my first time on doing this. Your product works really well - it could catch on for dashboard wood.
Rek
-
7 Years Ago
EC's NW1 cutting compound is far and above the best product I've ever used.
Hanaldo
-
7 Years Ago
OK -I will take a look Thanks
Rek
-
7 Years Ago
As Hanaldo states, NW1 White Super Cutting Compoundis the one we recommends as it works very well
Warren (Staff)
-
7 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search