Hi
I am wanting to create a mould from an item.
See picture.
This is a small sculpture, which is mounted to a front mudguard I created from the mould on the second picture.
I know I want to make the new mould in 2 pieces to allow creation of the shape and also allow release.
Any thoughts on the best areas to section this off to create the 2 halves?
Best regards
Steve
Attachments
IMG_0599.jpg (456 views, 1.00 MB)
IMG_0600.jpg (422 views, 1.00 MB)
Replies
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
nice one! i have a series 2 lammy so no good for GP bodywork!
I look forward to seeing what you are making

ojs technical
ojs technical
Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)
Group: Forum Members
Posts: 6, Visits: 90
scottracing - 4/18/2018 9:53:18 PM
nice one! i have a series 2 lammy so no good for GP bodywork!
I look forward to seeing what you are making

I do have some serI/II parts...I have a Winter Model and aim to make a full set of bodywork from kevlar composites....in due course.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
ojs technical - 7 Years Ago
Hanaldo - 7 Years Ago
scottracing - 7 Years Ago
ojs technical - 7 Years Ago
scottracing - 7 Years Ago
ojs technical - 7 Years Ago
scottracing - 7 Years Ago
ojs technical - 7 Years Ago
scottracing - 7 Years Ago
             no problem...will do...keep in touch
ojs technical - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search