Hi
I am wanting to create a mould from an item.
See picture.
This is a small sculpture, which is mounted to a front mudguard I created from the mould on the second picture.
I know I want to make the new mould in 2 pieces to allow creation of the shape and also allow release.
Any thoughts on the best areas to section this off to create the 2 halves?
Best regards
Steve
Attachments
IMG_0599.jpg (456 views, 1.00 MB)
IMG_0600.jpg (422 views, 1.00 MB)
Replies
ojs technical
ojs technical
Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)
Group: Forum Members
Posts: 6, Visits: 90
scottracing - 4/16/2018 10:59:16 AM
Looks like a vespa mudguard?

are you a detective?
:-)


yes its a T5 front mudguard. I have moulds and make a few.
I have been asked to make a mould with an addition. I pretty much know how I want shape it, but thought I would do the bright thing and ask for any other opinions.

Best regards

scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
ojs technical - 4/16/2018 8:17:40 PM
scottracing - 4/16/2018 10:59:16 AM
Looks like a vespa mudguard?

are you a detective?
:-)


yes its a T5 front mudguard. I have moulds and make a few.
I have been asked to make a mould with an addition. I pretty much know how I want shape it, but thought I would do the bright thing and ask for any other opinions.

Best regards


I currently own a p200e and have had a couple of px's before Smile trying to get the lambretta on the road this year too!

Is it a light fitting you are adding? I cant make out exactly what it is? But as Hanaldo says right down the middle would be best as long as you dont have any undercuts on the new shape you have added.


ojs technical
ojs technical
Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)
Group: Forum Members
Posts: 6, Visits: 90
scottracing - 4/16/2018 10:06:22 PM
ojs technical - 4/16/2018 8:17:40 PM
scottracing - 4/16/2018 10:59:16 AM
Looks like a vespa mudguard?

are you a detective?
:-)


yes its a T5 front mudguard. I have moulds and make a few.
I have been asked to make a mould with an addition. I pretty much know how I want shape it, but thought I would do the bright thing and ask for any other opinions.

Best regards


I currently own a p200e and have had a couple of px's before Smile trying to get the lambretta on the road this year too!

Is it a light fitting you are adding? I cant make out exactly what it is? But as Hanaldo says right down the middle would be best as long as you dont have any undercuts on the new shape you have added.


Hi
thanks for the reply.

I have one or two in the garage.
:-)
The fixture is actually structural......its an odd shape....I am making a couple for a local artist......

I have moulds for most Lambretta GP bodywork...a few vespa ones too....

I was aiming to go straight down the middle but wanted to canvas a bit of opinion....
Once its done I will post the pics.
Best regards Steve

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
ojs technical - 7 Years Ago
Hanaldo - 7 Years Ago
scottracing - 7 Years Ago
ojs technical - 7 Years Ago
scottracing - 7 Years Ago
ojs technical - 7 Years Ago
scottracing - 7 Years Ago
ojs technical - 7 Years Ago
scottracing - 7 Years Ago
             no problem...will do...keep in touch
ojs technical - 7 Years Ago