+x Warren (Staff) - 4/18/2018 1:20:29 PMI would use the ProFinish Carbon Fibre 2/2 Twill 3k 210g as you can make a template for each raised piece. You can then lay up each raised piece then drop over a flat piece of cloth with cut outs for the raised bits.