By Littlj01 - 4/18/2018 10:50:21 AM
I would like to skin a part of my dash board. I have purchased the necessary carbon kit form yourselves. But I do not know how to approach these particular bumps. Any advise before I start would be most welcome. Thanks in advance.
|
By Warren (Staff) - 4/18/2018 4:32:00 PM
Yes you could do it that way, it's just a bit more fiddly to get the fabric to stay where it is initially. Once it is stuck down to the tacky basecoat, don't coat it with clear resin yet - wait another few hours as the extra curing time will help hold the carbon in place a bit more.
|
|