Adding flanges to an aluminium mould


Author
Message
stuart321
stuart321
Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)
Group: Forum Members
Posts: 37, Visits: 178
I'm planning to reuse a sumpguard mould that was made for wet layup so doesn't have flanges for vac bagging.
I didn't want to weld the flanges on as it may distort the mould so instead I planned to usePU adhesive to attach the flanges leaving a small recess which I could then fill with silicon as IME epoxy resin doesn't release well from PU adhesive.

Any different views or advice before I do this?

Thanks
Stuart
Reply
stuart321
stuart321
Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)
Group: Forum Members
Posts: 37, Visits: 178
Yes - photo would help Whistling
As you can tell this mould hasn't been used for a couple of years and needs a good clean before anything but you can probably see it has 3 sides (f,l,r) with a small 60 degree flange and then just flat at the rear.  Epoxy sounds a good way to go as it leaves a smooth slippery finish - any other advice appreciated.

http://i1064.photobucket.com/albums/u379/sideways_stu/sg.jpg