Yes - photo would help Whistling
As you can tell this mould hasn't been used for a couple of years and needs a good clean before anything but you can probably see it has 3 sides (f,l,r) with a small 60 degree flange and then just flat at the rear.  Epoxy sounds a good way to go as it leaves a smooth slippery finish - any other advice appreciated.

http://i1064.photobucket.com/albums/u379/sideways_stu/sg.jpg
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Hi,

I assume that your flanges would also be made out of Aluminium, since you are talking about not welding them cos of distortion.

And since it would be a metal to metal bond, I would use epoxy glue. I always heard Matt saying PU was perfect for composite to composite bond, while epoxy would be a bit better for metal to metal, or composite to metal.

Maybe a couple pics of your mold / flanges would help us to figure it.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
stuart321
stuart321
Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)
Group: Forum Members
Posts: 37, Visits: 178
I'm planning to reuse a sumpguard mould that was made for wet layup so doesn't have flanges for vac bagging.
I didn't want to weld the flanges on as it may distort the mould so instead I planned to usePU adhesive to attach the flanges leaving a small recess which I could then fill with silicon as IME epoxy resin doesn't release well from PU adhesive.

Any different views or advice before I do this?

Thanks
Stuart