Group: Forum Members
Posts: 338,
Visits: 2K
|
Going back to one of your original questions regarding fabric, I think that you'll get better results using a 240g twill fabric, rather than Profinish
Profinish doesn't drape very well, owing to its binder. The 240g fabric is very stable, compared to the usual 200g twill and a mist of spray tack along your intended cut line will help to keep things very neat. The 240g is also tighter in its weave, so gives a similar appearance to pre-preg when laminated
|