I'm wanting to skin the top and bottom of a steering wheel in carbon fiber. I'm thinking about where I'll join the carbon fiber and whether I want to use the ProFinish carbon fiber or the regular stuff. I'd really like a neat cut line and joint. Also, it sounds like I might be able to get the weave alignment perfect more easily with the ProFinish. However, I'm wondering whether the ProFinish stuff is stiffer and less suited to wrapping around the rim of a steering wheel than the standard carbon fiber. 

Also, will the resin bond properly to the foam of a steering wheel core?
Would you recommend more than one layer of carbon fiber? My concern would be that one layer might crack if gripped too tightly. For what it's worth, the foam is fairly dense.
Any other tips or advice would also be very much appreciated.

Thanks,
Andrew
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
aforrister - 8 Years Ago
kidpaint - 8 Years Ago
Warren (Staff) - 8 Years Ago
aforrister - 8 Years Ago
MaksE55 - 8 Years Ago
Fasta - 8 Years Ago
aforrister - 8 Years Ago
kidpaint - 8 Years Ago
Fasta - 8 Years Ago
MaksE55 - 8 Years Ago
Hanaldo - 8 Years Ago
Fasta - 8 Years Ago
Fasta - 8 Years Ago
MarkMK - 8 Years Ago
kidpaint - 8 Years Ago
Fasta - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search