Hi Guys

Just  up dating my curing oven temp controller to a P I D controller. (Omega CN7823)
One of the functions is auto-tuning
My question is do i have to auto tune the pid every time i turn it on or is it a set up once type of thing !! tried ringing Omega but there tec guys i cant understand them because of there broken english language (other country)

Thanks for reading any help would be greatful


MarkMK
MarkMK
Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
Hi

I have an Omega 7800 series controller and I don't think that I've needed to perform any tuning work in the P.I.D function when programming multiple ramp cycles for curing various parts. In fact, I think that the process function when using the ramp/soak programme function is just a simple 'on/off' one. I could be wrong, though!

I too found both the tech support and manual a little bit unhelpful, so relied upon a bit of trial and error to get things working okay

The one thing that I do, however, is to attach a couple of external thermocouples to parts when in the oven to monitor temperature more closely from a fairly cheap reader. I found that having the single thermocouple at a fixed location in the oven connected to the controller was not giving an overly accurate picture and that the controller took some time whilst the oven fully 'warmed-up' to provide stable readings and close temperature control.