By carbon-bollox - 1/17/2018 5:38:58 PM
Hi Guys
Just up dating my curing oven temp controller to a P I D controller. (Omega CN7823) One of the functions is auto-tuning My question is do i have to auto tune the pid every time i turn it on or is it a set up once type of thing !! tried ringing Omega but there tec guys i cant understand them because of there broken english language (other country)
Thanks for reading any help would be greatful
|
By MarkMK - 1/22/2018 11:53:35 AM
Hi
I have an Omega 7800 series controller and I don't think that I've needed to perform any tuning work in the P.I.D function when programming multiple ramp cycles for curing various parts. In fact, I think that the process function when using the ramp/soak programme function is just a simple 'on/off' one. I could be wrong, though!
I too found both the tech support and manual a little bit unhelpful, so relied upon a bit of trial and error to get things working okay
The one thing that I do, however, is to attach a couple of external thermocouples to parts when in the oven to monitor temperature more closely from a fairly cheap reader. I found that having the single thermocouple at a fixed location in the oven connected to the controller was not giving an overly accurate picture and that the controller took some time whilst the oven fully 'warmed-up' to provide stable readings and close temperature control.
|
|