I'm making some fairly large panels for a motorcycle project for the full fairing, seat etc and so far have had pleasing results. I'm using three layers of 1x200 and 2x 450 carbon twill and resin infusion.
The moulds are multi part moulds made using the unimould system. Before laying up the carbon and bagging it I have applied four coats of easylease with 15-20 minutes between each and then a final fifth layer that is left for at least an hour before infusion.
I've watched Matt on all of the easycomposites videos demoulding parts and it looks effortless. Firstly when I'm removing the peel ply, it's really hard to do. Matt tears his in strips and it comes right off whereas I have to use all my strength to get it of free the carbon part and I'm no weakling! Then, where Matt's parts virtually pop out of the mould, mine need dozens of polypropylene wedges knocking into cracks to get it to come out. This Is largely, bar a few details, a flat panel and it takes me about 2 hours to free it.
On two of the five things I've made, part of the mould has come off with the part meaning major repairs if I wants to use the mould again.
I believe I've followed the instructions for easy lease to the letter but demoulding is a nightmare. What am I doing wrong or does Matt in the video just have superhuman finger strength?! Any suggestions appreciated as I'm about to move on to the complicated nose cone and want to get that out more easily. Thanks.
Reply
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
24 hours at room temperature is definitely far before the point of easiest release. But it should not be so difficult, that the tooling coat comes off. If this is not caused by geometrical issues, the easylease might be too old.
The peel ply comes off far more easy, if the resin is cured to a higher level. 48h at room temperature, even longer at usual workshop temperatures.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
moonpie - 7 Years Ago
Warren (Staff) - 7 Years Ago
moonpie - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
moonpie - 7 Years Ago
Warren (Staff) - 7 Years Ago
moonpie - 7 Years Ago
Finnluxury - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search